Grade : TT8080
PVD coated grade with optimum toughness for rough machining of steels, interrupted & rough machining of stainless steel and low speed & interrupted machining of heat-resistant alloys

PropertyValue
ISO Range - P/M/K(P30-P50)(M30-M50)
ISO Range - H/S/N (S30-S50)
HRA90
Coating TypePVD
Coating LayerTiAlN-TiN



Cutting Speed for: XNMU 0906 ANTR-M TT8080 - 6152533
ISOMaterialMaterial DescriptionMaterial ConditionCutting Speed Recommendations
P1Non-alloy steel and cast steel, free cutting steel <0.25%C.Annealed :125170-250 m/min
P2Non-alloy steel and cast steel, free cutting steel >=0.25%C.Annealed :190130-220 m/min
P3Non-alloy steel and cast steel, free cutting steel <0.55%C.Quench and tempered. :25090-170 m/min
P4Non-alloy steel and cast steel, free cutting steel >=0.55%C.Annealed :220100-190 m/min
P5Non-alloy steel and cast steel, free cutting steel >=0.55%C.Quenched & tempered. :30070-160 m/min
P6Low alloy & cast steel (less than 5% of alloying elements).Annealed :200150-220 m/min
P7Low alloy & cast steel (less than 5% of alloying elements).Quenched & tempered :275110-190 m/min
P8Low alloy & cast steel (less than 5% of alloying elements).Quenched & tempered :30080-160 m/min
P9Low alloy & cast steel (less than 5% of alloying elements).Quenched & tempered :35070-120 m/min
P10High alloyed steel, cast steel and tool steel.Annealed :20070-110 m/min
P11High alloyed steel, cast steel and tool steel.Quenched & tempered :32560-100 m/min
M12Stainless steel and cast steel.Ferritic/martensitic :20090-200 m/min
M13Stainless steel and cast steel.Martensitic :24070-160 m/min
M14Stainless steel and cast steel.Austenitic :180100-210 m/min
K15Grey cast iron (GG)Pearlitic/ferritic :180100-250 m/min
K16Grey cast iron (GG)Pearlitic/martensiti :26090-220 m/min
K17Nodular cast iron (GGG)Ferritic :160110-220 m/min
K18Nodular cast iron (GGG)Pearlitic :250130-200 m/min
K19Malleable cast iron.Ferritic :130150-250 m/min
K20Malleable cast iron.Pearlitic :230100-250 m/min
S31High temp. alloys Fe based.Annealed :20030-65 m/min
S32High temp. alloys Fe based.Cured :28020-45 m/min
S33High temp. alloys. Ni or Co based.Annealed :25025-50 m/min
S34High temp. alloys. Ni or Co based.Cured :35020-40 m/min
S35High temp. alloys. Ni or Co based.Castr :32020-45 m/min
S36Titanium (pure):31060-100 m/min
S37Titanium Ti alloys.Alpha+beta alloys cu :31025-55 m/min